Cargando…

Production of Electrolytic Composite Powder by Nickel Plating of Shredded Polyurethane Foam

Ni–poly(DPU) composite powder was produced under galvanostatic conditions from a nickel bath with the addition of pulverized polymer obtained during the shredding of polyurethane foam (poly(DPU)). The Ni–poly(DPU) composite powder was characterized by the presence of polymer particles covered with a...

Descripción completa

Detalles Bibliográficos
Autores principales: Niedbała, Jolanta, Popczyk, Magdalena, Hawełek, Łukasz, Orda, Szymon, Okła, Hubert, Gabor, Jadwiga, Stach, Sebastian, Swinarew, Andrzej S.