Fatigue Property and Small Crack Propagation Mechanism of MIG Welding Joint of 6005A-T6 Aluminum Alloy

In this study, metal inert gas welding (MIG) was applied to 4 mm thick 6005A-T6 aluminum alloy welding. Compared with other parts, the hardness of the weld zone (WZ) was the lowest, about 67 HV. There was the Softening in WZ, which might make WZ the weakest zone. Then, fatigue tests were carried out...