The Influence of Yb Doping and Sintering Conditions on the Magnetocaloric and Mechanical Properties of EuS

For this work, europium monosulfide (EuS) powders were prepared by sulfurizing Eu(2)O(3) powder with CS(2) gas. The synthesized EuS powders were sintered by SPS at temperatures in the 800–1600 °C range for 0.33–1 h at 50 MPa under vacuum conditions. The influences of Yb doping and sintering conditio...